Publication: Fracture Resistance and Failure Modes of Lithium Disilicate or Composite Endocrowns
dc.contributor.author | Altıer, Muhammed | |
dc.contributor.author | Erol, Funda | |
dc.contributor.author | Yıldırım, Gulhan | |
dc.contributor.author | DALKILIÇ, EVRİM | |
dc.contributor.institutionauthor | DALKILIÇ, EVRİM | |
dc.date.accessioned | 2020-10-30T00:34:06Z | |
dc.date.available | 2020-10-30T00:34:06Z | |
dc.date.issued | 2018-07-01T00:00:00Z | |
dc.description.abstract | Purpose: The aim of this study was to determine the fracture strength of endocrowns made of lithium disilicate ceramic and two different indirect resin composites. Materials and Methods: Forty human mandibular molars were randomly separated into four groups (n = 10 in each group) -Group IN: control group, Group IPS: endocrowns made of lithium disilicate ceramic (IPS e. max CAD, IvoclarVivadent, Schaan, Liechtenstein); Group SL: Endocrowns made of Solidex microhybrid composite (Shofu, Ratingen, Germany); and Group GR: Endocrowns made of Grandia microhybrid composite (GC Europa, Leuven, Belgium). In all of the groups, dual-cure resin cement (Relyx Ultimate Clicker, 3M ESPE, St. Paul, MN, USA) was used to cement the endocrowns. All of the teeth were subjected to fracture by means of a universal testing machine (Instron), and compressive force was applied. The failure type and location after fracture were classified. The data were analyzed using one-way ANOVA, Tukey-s post hoc test, and Chi-square test (P 0.05). In Group SL, 80% of the specimens exhibited favorable fractures; also, 60% of the specimens exhibited favorable fracture in group GR, and only 10% of the specimens exhibited favorable fracture in group IPS. Conclusions: The lithium disilicate ceramic endocrowns exhibited higher fracture resistance than indirect composite groups. Both of the composite endocrowns showed more favorable failure than the lithium disilicate ceramic endocrowns. | |
dc.identifier.citation | Altıer M., Erol F., Yıldırım G., DALKILIÇ E., -Fracture Resistance and Failure Modes of Lithium Disilicate or Composite Endocrowns-, NIGERIAN JOURNAL OF CLINICAL PRACTICE, cilt.21, ss.821-826, 2018 | |
dc.identifier.doi | 10.4103/njcp.njcp_175_17 | |
dc.identifier.pubmed | 29984710 | |
dc.identifier.scopus | 85050069802 | |
dc.identifier.uri | http://hdl.handle.net/20.500.12645/27261 | |
dc.identifier.uri | https://www.njcponline.com/article.asp?issn=1119-3077;year=2018;volume=21;issue=7;spage=821;epage=826;aulast=Altier | |
dc.identifier.wos | WOS:000439047000001 | |
dc.rights | info:eu-repo/semantics/openAccess | |
dc.subject | Fracture Resistance | |
dc.title | Fracture Resistance and Failure Modes of Lithium Disilicate or Composite Endocrowns | |
dc.type | Article | |
dspace.entity.type | Publication | |
local.avesis.id | fbf80960-e1c3-4a65-82d0-a05becdf1669 | |
local.indexed.at | PubMed | |
local.indexed.at | WOS | |
local.indexed.at | Scopus | |
local.publication.isinternational | 1 | |
relation.isAuthorOfPublication | 05592be3-8323-4273-bfff-96d4c4775aa8 | |
relation.isAuthorOfPublication.latestForDiscovery | 05592be3-8323-4273-bfff-96d4c4775aa8 |